"Far superior over the competition"

Tests for quality and overall coating performance were performed at Stonebridge Technical Services specializing in Automotive OEM Paint testing. Controlled laboratory testing proves dramatic superiority over the nearest competitor. Tests on Vecdör note a 53% improvement in scratch resistance over the closest competitor and 50-60% decrease in cleaning and surface maintenance when compared to other Automotive Aftermarket and Automotive OEM clear coatings.

Laboratory Tests note that Vecdör Clear Coating for Automotive has 75% better impact resistance, 476% better chemical resistance, and 45% better abrasion resistance than the closest automotive clear coat competitor.

"We have completed 4,000 hour weatherometer (WOM) testing of your Vecdör clearcoat. Vecdör was compared to the PPG® aftermarket CeramiClear® product and with the DuPont® OEM Acrylic Melamine clearcoat. Vecdör performed exceptionally well after 4,000 hours of WOM exposure. The Vecdör clearcoat showed superior cold temperature chip resistance, direct and reverse impact resistance compared to the CeramiClear® and DuPont® OEM clearcoats".

Stonebridge Technical Services - Debora Hense

» Vecdör Properties Test Report - Click

» Vecdör UV-WOM Test Report - Click

 


 

Compared to the PPG® aftermarket CeramiClear® product, Vecdör had superior abrasion resistance, scratch and gouge resistance, hardness, impact and MEK resistance. Vecdör outperformed the DuPont® OEM clearcoat in abrasion resistance, flexibility and impact resistance.

Stonebridge Technical Services - Debora Hense

» 4000 hour weatherometer: 100% gloss retention
» ASTM D3363 pencil hardness: 6H
» Amtec Kistler - Car Wash Test: 96% gloss retention
» Crockmeter test: 97% gloss retention
» Tukon hardness: 11.4
» ASTM D524 gloss (20¡/60¡): 90.2
» ASTM D3359 adhesion test method B: 5B/100%
» ASTM D4060 abrasion resistance: 19.58g
» ASTM D4752 MEK resistance: Greater than 1500
» ASTM D1308 chemical spot resistance: no effect
» ASTM D1308 skydrol immersion (7 days): no effect
» ASTM D522 flexibility test: 0-T
» ASTM D2794 impact resistance direct: 140 pass
» ASTM B117 salt spray test method: 3000 hours
» Water contact degree angle: 90
» ASTM D4585 humidity resistance: no effect
» ASTM D3170 chip resistance: 7A
» ASTM D968 falling sand abrasion (100 liters): pass

 


Water Drag Resistance Test Results

Coming Soon


Questions? (877) 998-3737

Email: question@nanovere.com

 
Copyright © 2007 Nanovere Technologies, LLC.
All Rights Reserved
Home | About Us | Vecdör Nanocoatings | University Testing | Customer Testimonials | Licensing Opportunities | Contact Us